A Viscoplastic Model Based on a Variable Strain Rate Sensitivity Index for Superplastic Sheet Metals
In recent years, superplastic forming (SPF) technology has been used for producing complex sheet components in automotive and aerospace industries. Under the SPF conditions, i.e. low strain rates and elevated temperatures, a superior elongation is achieved.