Anomalous bulging behaviors of a dielectric elastomer balloon under internal pressure and electric actuation

Submitted by tongqing.lu on

When a clamped membrane of elastomer is subject to a lateral pressure, it bulges into a hemispherical balloon. However, for a clamped membrane of dielectric elastomer (DE) under a lateral pressure as well as a voltage through the thickness, it may bulge into a regular hemispherical balloon or an irregular shape. This work focuses on the anomalous bulging behaviors (i.e. the irregular bulging shape) of a DE balloon under electromechanical coupling loading.

orthotropic

Submitted by vbabbas on

hello all.

I work on the plates laminate orthotropic, in the calculation of the constatnte of rigidities I found two matrices of rigidity which are mantionent on the two figures following:

somebody can explain to me which is the matrix right, and thank you by advance.

PhD positions in mechanics of metamaterials at the University of Minnesota

Submitted by stefanogonella on

PhD positions are available at the University of Minnesota in the group of Prof. Stefano Gonella. The positions are in the general area of mechanics and physics of solids and structures, with emphasis on mechanical metamaterials. Topics of current interest are:

1) Topological metamaterials;

2) Nonlinear waves in metamaterials and architected solids;

3) Tunable and programmable metastructures.

Experimentally informed micromechanical modelling of cement paste: An approach coupling X-ray computed tomography and statistical nanoindentation

Submitted by shavijabranko on

Our group has recently published an article wherein we propose the use of X-ray computed tomography coupled with statistical nanoindentation for simulating the mechanical properties of quasi-brittle materials. The approach is used for simulating tensile properties of hardened cement paste.