Nonlinear mechanics of phase-change-induced accretion
In this paper, we formulate a continuum theory of solidification within the context of finite-strain coupled thermoelasticity. We aim to fill a gap in the existing literature, as the existing studies on solidification typically decouple the thermal problem (the classical Stefan's problem) from the elasticity problem, and often limit themselves to linear elasticity with small strains.