Skip to main content

microstructure

Postdoc seeking in field of Mechanical or Materials Science Engineering

Submitted by lifeiwang on

My name is Lifei Wang, from China. I am 28 years old, and I have been finished my P.H.D degree in July 2015.   Now I'm looking for a postdoc research position in the field of Mechanical or Material Science Engineering. 

Mechanical, microstructural and fracture properties of dissimilar welds produced by friction stir welding of AZ31B and Al6061

Submitted by a.dorbane on

Friction stir welding (FSW) has been used for joining AZ31B magnesium alloy and Al 6061-T6 aluminum alloy sheets. In this regard, the current work aims to study the mechanical, microstructural and fracture properties of dissimilar FSW welds obtained by evolving the tool rotation and translation speeds. The dissimilar welds microstructure and mechanical properties are evaluated and correlated with the FSW parameters to obtain the optimum weld conditions. The results showed that placing aluminum on the advancing side of the weld resulted in better quality welds.

Temperature induced crack propagation in structured media

Submitted by Giorgio Carta on

This paper describes the propagation of an edge crack in a semi-infi nite triangular lattice, consisting of identical point masses connected by thermoelastic links. A change of temperature, represented by a time-periodic series of high-gradient temperature pulses, is applied at the boundary of the lattice. In order to make the initial crack advance in the lattice a failure criterion is imposed, whereby the links break as soon as they attain a prescribed elongation.

PhD position in Analysis of Fracture in Porous Ceramic Catalysts by use of X-ray Tomography

Submitted by hlfrandsen on
The Department of Energy Conversion and Storage at the Technical University of Denmark (DTU) and Haldor Topsøe A/S (HTAS) is seeking a candidate for a PhD position in analysis of fracture in porous ceramic steam-reforming catalysts by use of X-ray tomography.
 
Responsibilities and tasks


Finite Element software Z-set : new web page

Submitted by Vladislav Yastrebov on

New web page of Finite Element Analysis software Z-set is now open: http://zset-software.com/

What is Z-set

Z-set is a computational code devoted to the analysis of material and
structure behavior, involving a finite element solver and a collection
of specific tools for material parameter calibration, preprocessing and
postprocessing computations. Z-set is the result of 30 years of close collaboration between the

Analysis of microstructural induced enhancement of electromechanical coupling in soft dielectrics

Submitted by Stephan Rudykh on

Electroactive soft elastomers require huge electric field for a meaningful actuation. We demonstrate, by means of numerical simulation, that this can be dramatically reduced and large deformations can be achieved with suitably designed heterogeneous actuators. The mechanism by which the enhancement is attained is illustrated with the aid of both idealized and periodic models.

3-D Microstructure Reconstruction of Polymer Nano-Composite using FIB-SEM and Statistical Correlation Function

Submitted by Azadeh Sheidaei on

 http://www.sciencedirect.com/science/article/pii/S0266353813001012?np=y

Abstract

3-D
reconstruction of Halloysite nanotube (HNT) polypropylene composite has
been performed using two different methods. In the first method,
several slices of the composite material were obtained using focused ion
beam (FIB), and scanning electron microscopy (SEM). A representative
volume element (RVE) of the real material’s micro/nanostructures was